1996
Book Article
Title

Single-sintered PM connecting rods

Other Title
Sinterpleuel, hergestellt in der Einfachsintertechnik
Abstract
The single sintering technique with densities around 7.1 g/cm3 is able to cover the needs of 1.5 to 2.0 l engines up to 7,000 rpm and promises, fracture splitting of the big bore provided, a very economic and reliable alternative with the advantage of guaranteed minimum weight scatter below +-5g and dimensional accuracy.
Author(s)
Richter, K.
Hoffmann, E.
Lipp, K.  
Sonsino, C.M.  
Fraunhofer-Institut für Betriebsfestigkeit und Systemzuverlässigkeit LBF  
Mainwork
Automotive Manufacturing International 1996  
Language
English
Fraunhofer-Institut für Betriebsfestigkeit und Systemzuverlässigkeit LBF  
Keyword(s)
  • connecting rod

  • Dauerfestigkeit

  • endurance limit

  • heat treatment

  • Konstruktion

  • sintered steel

  • Sinterpleuel

  • Sinterstahl

  • structure

  • Wärmebehandlung