Options
2010
Conference Paper
Title
Sintering of nanostructured WC-10Co/316L stainless-steel composite parts made by assembling of the PIM parts
Abstract
This paper reports co-sintering response of nanostructured WC-Co/316L stainless steel composite produced by assembling of powder injection molding (PIM) parts. A significant mismatch sintering shrinkage (>4%) was observed in the temperature range of 1080-1350 °C. The reaction between WC and Fe at the contact area resulted in the diffusion of C and Co into the iron lattice and eventually formation of a low-temperature liquid phase that in fact affects the shape control of the PIM parts during sintering. In order to make the co-sintering feasible, a special sintering cycle was developed. The reaction between the cemented carbide and stainless steel was also retarded by developing a special Ni-W past. This articles presents a protocol to fabricate WC/316L composite structures by powder injection molding process. Such a composite structure is practically very useful because only a part of the article is made from cemented carbides to yield wear resistance while the rest is manufactured from a cheaper metal with an aim of cost reduction and/or to provide a function, for example, corrosion resistance.