Under CopyrightBlug, AndreasAndreasBlugKoss, Peter A.Peter A.KossDurmaz, Ali RizaAli RizaDurmazLaskin, GennadiiGennadiiLaskinBertz, AlexanderAlexanderBertzKühnemann, FrankFrankKühnemannStraub, ThomasThomasStraub2022-03-159.10.20219.10.20212021https://publica.fraunhofer.de/handle/publica/41249810.24406/publica-fhg-412498Magnetic and magneto-mechanical testing are commonly used for qualitative characterization of damage in devices and in large test sites. This presentation reports first results obtained with an optically pumped zero-field magnetometer (OPM) in combination with a micro fatigue setup. The small sample volume of about 1 mm³ allows metallographic characterization of specific material defects occurring during the fatigue process and linking them to features in the magnetic signal.enOptically Pumped Magnetometersfatigue testingMagneto-Mechanical Hysteresis620621Measuring Magneto-Mechanical Hysteresis during Fatigue Testing using Optically Pumped Magnetometersposter