Options
2027
Journal Article
Title
From fibre to composite: Mechanical performance of unidirectional GFRP materials based on novel high-modulus glass fibres
Abstract
Increasing blade lengths in the wind-energy sector push E-glass fibre-reinforced polymers (E-GFRP) to their ultimate stiffness limit. High-modulus glass fibres (HM-GF) based on the MgO-Al2O3-SiO2 glass system (MAS), modified with Y2O3 and ZnO, have been characterised at bulk-glass and single-fibre level in prior work, but their composite-level performance, the decisive criterion for application, remains unexplored. Here, unidirectional GFRP rods (DIN EN ISO 9163) and vacuum-infused UD laminates were manufactured from self-drawn E-glass fibres (E-GF) as reference and from HM-GF (V10: MAS + 7 wt% Y2O3 + 7 wt% ZnO) using two epoxy matrices. Tensile (DIN EN 2747) and three-point bending (DIN EN ISO 14125) behaviour was determined. At rod level (an indicative screening step), V10-GFRP reaches +90.6 % tensile strength and +22.0 % modulus over the E-glass based reference samples. At UD-laminate level, it shows +63.2 % tensile strength, +56.6 % tensile modulus, +51.8 % flexural strength and +48.4 % flexural modulus. A rule-of-mixtures and Halpin–Tsai analysis yields a micromechanical lamina property set (E1 measured; E2, G12 model-derived), from which classical laminate theory predicts that the modulus gain is largely retained in 0°-dominated laminates (+40 % for [0/90]s) but diminishes in shear-dominated lay-ups. At iso-bending-stiffness, the UD modulus gain corresponds to a first-order ≈ 14 % skin-thickness reduction (a stiffness-equivalent upper-bound estimate that neglects strength, buckling, fatigue, density and safety factors), providing an indicative basis for MAS-based HM-GF in next-generation blade sections and beyond.
Author(s)
Open Access
File(s)
Rights
CC BY 4.0: Creative Commons Attribution
Additional link
Language
English