  4. Non-destructive monitoring of polymer degradation in PV modules by compressive stress relaxation measurement and implications for the PV module reliability
 
  • Details
  • Full
Options
2026
Journal Article
Title

Non-destructive monitoring of polymer degradation in PV modules by compressive stress relaxation measurement and implications for the PV module reliability

Abstract
The initial non-destructive lamination control of photovoltaic (PV) modules is indispensable to ensure enhanced reliability and lifetime. Compressive stress relaxation measurement (CSRM) is most commonly used for this purpose. This work focuses on the use of the CSRM as a monitoring method for PV modules during weathering. Therefore, PV modules with varying degrees of lamination were exposed to damp heat (DH) and damp heat with additional UV-irradiation (DH+UV). During the CSRM, the mechanical properties of the encapsulation and the backsheet are measured simultaneously. To decouple microstructural changes of the encapsulant and the backsheet, the CSRM was supplemented by swelling experiments. Swelling experiments can be used to calculate cross-linking density, making them a superior alternative to the Soxhlet method. Additionally, differential scanning calorimetry (DSC) was used to investigate the melting and crystallisation behaviour of the encapsulant and the backsheet. After the first 250 h of the DH test, the encapsulants showed an increase in the degree of cross-linking but maintained differences between the samples throughout the test. As a result, the PV module power degradation had a correlation with the initial cross-linking state. By the end of the test, the encapsulant and the backsheet had degraded, resulting in a drop of the CSRM response. The cross-linking density decreased in the encapsulant, while the backsheet underwent post-crystallisation and showed chain scission. The combined DH+UV weathering test caused post-cross-linking within the first 250 h, leading to levelling of the cross-linking states. The cancelled chemical differences in the encapsulants became reflected in a similar module power degradation. Thus, overacceleration shall be avoided by all means to deliver realistic reliability predictions.
Author(s)
Wessel, Patrick
Fraunhofer-Institut für Mikrostruktur von Werkstoffen und Systemen IMWS  
Gottschalg, Ralph
Fraunhofer-Institut für Mikrostruktur von Werkstoffen und Systemen IMWS  
Mordvinkin, Anton
Fraunhofer-Institut für Mikrostruktur von Werkstoffen und Systemen IMWS  
Journal
Polymer Testing
Funder
Bundesministerium für Wirtschaft und Klimaschutz  
Open Access
File(s)
Download (1.84 MB)
Rights
CC BY 4.0: Creative Commons Attribution
DOI
10.1016/j.polymertesting.2026.109345
10.24406/publica-10943
Additional link
Full text
Language
English
Fraunhofer-Institut für Mikrostruktur von Werkstoffen und Systemen IMWS  
Keyword(s)
  • Compressive stress relaxation measurement

  • Cross-linking density

  • Gel content

  • Lamination

  • Photovoltaic module reliability

  • Post-cross-linking