Einfluß des Kohlenstoffgehalts, der Vorverformung und der Korngröße von Kohlenstoffstählen auf die inhomogene Scherverformung

 
: Pintat, T.; Scholz, B.; Kunze, H.-D.; Vöhringer, O.

2nd Defence Research Group Seminar '88. Proceedings
1988
North Atlantic Treaty Organization (Tagung) <2, 1988, Bremen>
Deutsch
Konferenzbeitrag
Fraunhofer IFAM ()
adiabatic; carbon; energy; grain; inhomogeneous; predeformation; shearing; strainrate; work

Abstract
The work of deformation or energy consumption during shearing of two plain carbon steels with 0.1 wt% and 0.45 wt% carbon was determined as a function of strain rate. The steel with 0.1 wt% carbon was predeformed by swaging. A predeformation leads to minor energy consumption. The grain size of the steel with 0.45 wt% carbon was varied by different annealing treatments. The work of deformation increase with rising grain size. This effect seems to be initiated by Lüders strain. In the steel Ck 10 only homogeneous shearing or deformation shear zones could be observed, while in the steel Ck 45 transformation shear zones occured additionally.